A Stepbystep Guide to the Zinc Electroplating Process ...
The process of cleaning an object involves two steps: alkaline bath and electrocleaning. Soaking the metal in an alkaline bath for 5 – 10 minutes, at about 150° F is usually enough to get rid of most of the soil and dirt. After this, the parts are cleaned further in an electrocleaner. An electric charge is applied to the metal either at its ...